Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 19.0 microns | 0.750 mil | Adhesive |
Dielectric Polymers NT-4502 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |
|||
Thickness | 19.0 microns | 0.750 mil | |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 2 |
Arlon R3313X016-38 0.0165" (0.419 mm) Cured Silicone Rubber with Fiberglass Substrate 38" Wide
(dis Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 1 |
Arlon R3313X016-38 0.0165" (0.419 mm) Cured Silicone Rubber with Fiberglass Substrate 38" Wide
(dis Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 19.0 microns | 0.750 mil | |
Honeywell Capran® Unidraw (0.75 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 0.75 mil (19 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |
|||
Thickness | 19.0 microns | 0.750 mil | |
Honeywell Capran® Oxyshield™ M-OPA (0.75 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Thickness | 19.0 - 23.0 microns | 0.748 - 0.906 mil | |
Isoflon Polyester film Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). .. |
|||
Thickness | 19.0 microns | 0.750 mil | |
Formosa Plastics Formolene® E922 Film HDPE High Density Polyethylene Medium Molecular Weight Bi-Modal Resin Designed for Film Applications Formolene® E922 is a medium molecular weight grade of HDPE designed for good processing characteristi.. |
|||
Thickness | 19.0 microns | 0.750 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 75 AB-X OPP Film Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as.. |
|||
Thickness | 19.0 microns | 0.750 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 75 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Thickness | 19.0 microns | 0.750 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 75 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Thickness | 19.0 microns | 0.750 mil | ExxonMobil Method |
ExxonMobil Bicor™ 19MB440 OPP Film Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America.. |
|||
Thickness | 19.0 microns | 0.750 mil | |
Dow DAF 780 Carpet Underlayment Adhesion Film DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow |
|||
Thickness | 19.0 microns | 0.750 mil | |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Thickness | 19.0 microns | 0.750 mil | |
Dow Saran® 18L Clear Plastic Barrier Film Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow |
|||
Thickness | 19.0 microns | 0.750 mil | |
Dow Saran® 18L-WP White Plastic Barrier Film Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow |
|||
Thickness | 19.0 microns | 0.750 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 1, Cured Layer; Arlon SQA-TMS-003 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Uncured Silicone Rubber Substrate: Style 7628 FiberglassSide 2: Cured Silicone RubberAppearan.. |
|||
Thickness | 19.0 microns | 0.750 mil | side 1, layer 1 cured silicone; Arlon SQA-TMS-003 |
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 19.0 microns | 0.750 mil | side 2; Arlon SQA-TMS-003 |
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 19.0 microns | 0.750 mil | side 1/cured; Arlon SQA-TMS-003 |
Arlon 51228R025 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 19.0 microns | 0.750 mil | Backside Adhesive |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Thickness | 19.0 microns | 0.750 mil | Side 1, Cured Layer; Arlon SQA-TMS-003 |
Arlon R35928R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R35928R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 19.0 microns | 0.750 mil | Backside Adhesive |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Thickness | 19.0 microns | 0.750 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 19.0 microns | 0.750 mil | Side 1, Cured Layer; Arlon SQA-TMS-003 |
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 19.0 microns | 0.750 mil | Adhesive |
Dielectric Polymers NT-5002 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |