Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® E922 Film HDPE

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® E922 Film HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Density Polyethylene Medium Molecular Weight Bi-Modal Resin Designed for Film Applications Formolene® E922 is a medium molecular weight grade of HDPE designed for good processing characteristics and good film stiffness for thin gauge film applications. Formolene® E922 meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Applications: Shopping Bags, Trash Can Liners and Thin Film for Laminate ApplicationsInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Thickness 19.0 microns
0.750 mil
Melt Flow 0.15 g/10 min
0.15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 390 %
390 %
ASTM D882
Film Elongation at Break, TD 640 %
640 %
ASTM D882
Elmendorf Tear Strength MD 13 g
13 g
ASTM D1922
Elmendorf Tear Strength TD 220 g
220 g
ASTM D1922
Dart Drop Test 240 g
0.529 lb
ASTM D1709
Film Tensile Strength at Break, MD 51.7 MPa
7500 psi
ASTM D882
Film Tensile Strength at Break, TD 52.4 MPa
7600 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 132 °C
270 °F
DSC
Processing Properties Metric English Comments
Blow-up Ratio (BUR) 4.0
4.0