Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.5 - 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 - 4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM 353B General Purpose Polystyrene Grade 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. It is used for electronic packaging, extruded light diffusers and office accessories.Informa.. |
|||
Melt Flow | 2.5 - 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.5 - 4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM 535 General Purpose Polystyrene Grade 535 is a high heat crystal polystyrene designed for injection molding, extrusion and blow molding. It is used for electronic packaging, extruded light diffusers and office accessories.Informa.. |
|||
Melt Flow | 2.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Bio-Flex® F 6510 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melt Flow | 2.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238-04 |
Ineos H03BLME Polypropylene Homopolymer This is a homopolymer designed for extrusion, and it is compliant with both the FDA status 21CFR 177.1520(C) 1.1 and the EU Food Contact status 2002/72/EC.Information provided by Ineos Olefins & Pol.. |
|||
Melt Flow | 2.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238-04 |
Ineos H03SLME Polypropylene Homopolymer This is a homopolymer designed for extrusion, and it is compliant with both the FDA status and the EU Food Contact status.Information provided by Ineos Olefins & Polymers USA |
|||
Melt Flow | 2.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238-04 |
Ineos H03YLME Polypropylene Homopolymer This is a homopolymer designed for extrusion, and it is compliant with both the FDA status and the EU Food Contact status.Information provided by Ineos Olefins & Polymers USA |
|||
Melt Flow | 0.50 - 4.5 g/10 min | 0.50 - 4.5 g/10 min | |
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist.. |
|||
Melt Flow | 2.0 - 4.5 g/10 min @Load 10.0 kg, Temperature 230 °C |
2.0 - 4.5 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF) Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3.. |
|||
Melt Flow | 3.8 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.8 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) Arak 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 3.8 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.8 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) Tabriz 0640AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |