Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 81.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
81.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Melt Flow | 81.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
81.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Melt Flow | 81.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
81.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Melt Flow | 81.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
81.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Melt Flow | 81.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
81.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Melt Flow | 81.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
81.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |