Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.00 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.00 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D123 |
Niche Polymer ABSN3BK ABS Information provided by Niche Polymer |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1166B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2150 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2249 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 1.00 kg, Temperature 235 °C |
8.00 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1358D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-4123 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene CPP1050 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene MFP 22KA2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1267A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2540A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2540F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 8.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |