Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.00 - 236 g/10 min | 3.00 - 236 g/10 min | Average value: 35.8 g/10 min Grade Count:92 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Melt Flow | 3.00 - 82.0 g/10 min | 3.00 - 82.0 g/10 min | Average value: 27.0 g/10 min Grade Count:35 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Melt Flow | 3.00 - 35.0 g/10 min | 3.00 - 35.0 g/10 min | Average value: 15.6 g/10 min Grade Count:11 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melt Flow | 3.00 - 46.0 g/10 min | 3.00 - 46.0 g/10 min | Average value: 14.0 g/10 min Grade Count:102 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 8.86 g/10 min Grade Count:38 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 11.6 g/10 min Grade Count:9 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Melt Flow | 3.00 - 44.0 g/10 min | 3.00 - 44.0 g/10 min | Average value: 15.4 g/10 min Grade Count:106 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Melt Flow | 3.00 - 56.0 g/10 min | 3.00 - 56.0 g/10 min | Average value: 16.6 g/10 min Grade Count:41 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Melt Flow | 3.00 - 115 g/10 min | 3.00 - 115 g/10 min | Average value: 39.2 g/10 min Grade Count:21 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Melt Flow | 3.00 - 81.6 g/10 min | 3.00 - 81.6 g/10 min | Average value: 43.7 g/10 min Grade Count:21 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Melt Flow | 3.00 - 33.0 g/10 min | 3.00 - 33.0 g/10 min | Average value: 19.0 g/10 min Grade Count:5 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melt Flow | 3.00 - 60.0 g/10 min | 3.00 - 60.0 g/10 min | Average value: 25.9 g/10 min Grade Count:10 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Flow | 3.00 - 50.0 g/10 min | 3.00 - 50.0 g/10 min | Average value: 9.70 g/10 min Grade Count:8 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Flow | 3.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Melt Flow | 3.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1881 Thermoplastic Elastomer Uses: Grips Features: Excellent Resistance to Skin OilsInformation Provided by Teknor Apex |
|||
Melt Flow | 3.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2189 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 3.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 3.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 1934G Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Melt Flow | 3.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1097F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 3.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1205A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 3.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 3.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-4001A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 3.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Melt Flow | 3.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Melt Flow | 3.00 - 50.0 g/10 min | 3.00 - 50.0 g/10 min | Average value: 17.4 g/10 min Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Melt Flow | 3.00 - 25.0 g/10 min | 3.00 - 25.0 g/10 min | Average value: 9.65 g/10 min Grade Count:10 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Flow | 3.00 - 45.0 g/10 min | 3.00 - 45.0 g/10 min | Average value: 13.8 g/10 min Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Melt Flow | 3.00 g/10 min @Load 10.0 kg, Temperature 190 °C |
3.00 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinelec CCB1861 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Films; Packaging Forms: Pellets Processing Method: Blown FilmInformation Provid.. |