Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 81 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 130HF Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI 10 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents. Main application fields: autom.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
LyondellBasell Ultrathene® UE624000 Ethyl Vinyl Acetate Copolymer ApplicationsUltrathene UE 624-000 is an ethylene vinyl acetate (EVA) copolymer typically used as a base resin for highly filled compounds.This product is from the former Equistar product line. |
|||
Melt Flow | 2.2 - 2.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 - 2.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ISO 1133 |
Lucite International Diakon® CMG334V Acrylic Polymer Information provided by Lucite International |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ISO 1133 |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced WNP GradeInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 800 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SH 2114 High Impact Polystyrene Characteristics Very high impact strength Easy processing High heat Processing Extrusion MoldingApplications Toys, shoe heels, cosmetic boxes, pill vials Luggage cases Blending with clear polys.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EP310 Low Density Polyethylene WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips MarFlex® 5429 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Excellent openabilitySuited for high speed convertingGood clarityMedium coefficient of frictionTypical cast film applications include:Co.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips MarFlex® 5430 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Excellent opticsEasy processingHigh coefficient of frictionTypical cast film applications include:OverwrapCoextruded filmGeneral purpose.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips MarFlex® 5440 Low Density Polyethylene, Cast Film This LDPE is tailored for cast film applications that require:Suited for high speed convertingGood clarityLow coefficient of frictionTypical cast film applications include:Coextruded filmGeneral pur.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Exxon Method |
ExxonMobil EXACT™ 4053 Cast Plastomer Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Condition D; ASTM D 1238 |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem TS9022 Blown Film Extrusion Low Density Polyethylene Films for automatic overwrap packaging of hygiene markets. Typical applications are toilet tissue, kitchen paper and napkin (paper product) overwrap. Films which require good optical properties al.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem IH57 HDPE Injection Molding Polyethylene Copolymer IH57 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stress cracking resistance with pr.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade Bapolene PP4022 is a PP homopolymer designed for oriented film applications. It offers good clarity and optical properties. This resin meets FDA standards for food contact applications.Application.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
Huntsman Rexell® M3105 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of toughness, stiffness, and water vapor barrier with good temperature resistance.Applications:.. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 80 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Condition G |
Ineos Nova 5490 High Impact Polystyrene
(discontinued **) High heat, Good environmental stress crack resistance, Excellent printabilityApplications: Custom sheet, Lithographic applicationsProperties were determined on injection molded specimens at 23°C an.. |