Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.8 g/10 min @Load 5.00 kg, Temperature 280 °C |
13.8 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Melt Flow | 13.8 g/10 min @Load 5.00 kg, Temperature 280 °C |
13.8 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Melt Flow | 13.8 g/10 min @Load 5.00 kg, Temperature 280 °C |
13.8 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Melt Flow | 13.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® XG5858 TPC-ET Injection Molding |
|||
Melt Flow | 13.8 g/10 min @Load 2.16 kg, Temperature 125 °C |
13.8 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Dow Primacor® 5986 Ethylene acrylic acid copolymer Low heat seal temperature High gloss, excellent clarity Excellent grease and oil resistance and excellent product resistance for flexible packaging applications Complies with U.S. FDA 21 CFR 177.131.. |