Physical Properties Metric English Comments
Melt Flow 1.50 - 120 g/10 min
1.50 - 120 g/10 min
Average value: 12.7 g/10 min Grade Count:74
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Melt Flow 1.50 g/10 min

@Load 10.0 kg,
Temperature 190 °C
1.50 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex HFFR 2005 Polyolefin, Halogen Free
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable JacketingAgency Ratings: IEC Unsp..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP 1627L3 Thermoplastic Elastomer
Features: Excellent Elastic Recovery; Tough; Good Melt Strength Uses: Strap ProductsInformation Provided by Teknor Apex
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 3005L3 Thermoplastic Elastomer
Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1500SC Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1566L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1627 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2156 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2156-L1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2290 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2336UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2740 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2740L3-UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2740UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2850E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4470A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-101 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1336 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2596C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Uniprene® UN-1373G Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Flow 1.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Uniprene® UN-7100-50D Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 1245A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 1566 Thermoplastic Elastomer
Notes: Translucent Features: Super Tough; Excellent Melt Strength; Good Chemical and Oil ResistanceInformation Provided by Teknor Apex
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2579B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 1.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-3005 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..