Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.900 - 99.0 g/10 min | 0.900 - 99.0 g/10 min | Average value: 8.02 g/10 min Grade Count:409 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Flow | 0.900 - 16.9 g/10 min | 0.900 - 16.9 g/10 min | Average value: 7.80 g/10 min Grade Count:3 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 0.900 - 19.0 g/10 min | 0.900 - 19.0 g/10 min | Average value: 3.77 g/10 min Grade Count:17 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Flow | 0.900 - 70.0 g/10 min | 0.900 - 70.0 g/10 min | Average value: 13.9 g/10 min Grade Count:61 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Melt Flow | 0.900 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.900 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Melt Flow | 0.900 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.900 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 0.900 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.900 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 0.900 - 16.0 g/10 min | 0.900 - 16.0 g/10 min | Average value: 7.14 g/10 min Grade Count:17 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |