Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.100 - 10.0 g/10 min | 0.100 - 10.0 g/10 min | Average value: 3.44 g/10 min Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 0.200 - 10.0 g/10 min | 0.200 - 10.0 g/10 min | Average value: 1.86 g/10 min Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 0.200 - 10.0 g/10 min | 0.200 - 10.0 g/10 min | Average value: 3.72 g/10 min Grade Count:14 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Melt Flow | 1.00 - 10.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
1.00 - 10.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB3131 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 2.50 - 10.0 g/10 min | 2.50 - 10.0 g/10 min | Average value: 4.50 g/10 min Grade Count:4 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 2.50 - 10.0 g/10 min | 2.50 - 10.0 g/10 min | Average value: 5.43 g/10 min Grade Count:7 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |