Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.00 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.00 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D123 |
Niche Polymer ABSN3BK ABS Information provided by Niche Polymer |
|||
Melt Flow | 8.00 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.00 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D123 |
Niche Polymer ABSN4BK ABS Information provided by Niche Polymer |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1166B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2120 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2249 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 8.00 g/10 min @Load 1.00 kg, Temperature 235 °C |
8.00 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Melt Flow | 8.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1755L3 Thermoplastic Elastomer Notes: USP Class VI; ISO 10993 Features: Silken Feel; Tough; Good Melt Strength Uses: Medical BulbsInformation Provided by Teknor Apex |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene MFP 22KA2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1267A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 8.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2588L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-F.. |
|||
Melt Flow | 8.00 - 160 g/10 min | 8.00 - 160 g/10 min | Average value: 39.9 g/10 min Grade Count:22 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Melt Flow | 8.00 - 130 g/10 min | 8.00 - 130 g/10 min | Average value: 64.2 g/10 min Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Melt Flow | 8.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |