Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 30.0 g/10 min | 5.00 - 30.0 g/10 min | Average value: 11.6 g/10 min Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Melt Flow | 5.00 - 50.0 g/10 min | 5.00 - 50.0 g/10 min | Average value: 20.0 g/10 min Grade Count:6 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Flow | 5.00 - 17.0 g/10 min | 5.00 - 17.0 g/10 min | Average value: 9.67 g/10 min Grade Count:9 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Melt Flow | 5.00 - 70.8 g/10 min | 5.00 - 70.8 g/10 min | Average value: 37.9 g/10 min Grade Count:4 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1061 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 2860E Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1888 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1907E CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 8313 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1227A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2455 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 21.6 kg, Temperature 200 °C |
5.00 g/10 min @Load 47.6 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2666 Acrylonitrile Butadiene Styrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (200000 ppm) Uses: Sheet Forms: Pellets Processing Method: Injection Molding; Sheet ExtrusionI.. |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1332 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: High Gloss Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 - 20.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 20.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW3422 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL EF-6133L2 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1477B AUTO UV BLACK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2439D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2460B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2470A Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2420A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low .. |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1322 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) Forms: Pellets Features: General PurposeInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 - 130 g/10 min | 5.00 - 130 g/10 min | Average value: 28.1 g/10 min Grade Count:50 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Flow | 5.00 - 21.0 g/10 min | 5.00 - 21.0 g/10 min | Average value: 15.0 g/10 min Grade Count:10 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |