Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 25 g/10 min @Load 0.325 kg, Temperature 270 °C |
25 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP600R Injection Grade Polypropylene Moplen HP600R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600R is a homopolymer typically used in injection molding of food.. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® OQ3120 PC High Flow. UV-stabilized. Inherent mold release. Ophthalmic lenses. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® OQ4120R PC Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets. MFR of 25. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
25 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 220 °C |
25 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® LGA-SF
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir.. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 330 °C |
25 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 330 °C |
25 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
Hyosung Topilene J740 PP J740 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporation.. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
Hyosung Topilene J742 PP J742 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporat.. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 230 °C |
25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-9522 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9522 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9522 is dev.. |
|||
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 220 °C |
25 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Styrolution NOVODUR® P2MC ABS, Injection Grade Injection molding grade for plating; very good ratio between toughness, heat resistance and flow.Applications: All parts to plating: e.g. sanitary parts. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 250 °C |
25 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Triloy® 225 PC/ABS alloy Characteristics:Impact resistantHeat resistantDimensional stabilityApplications:Air con. grillAll information provided by Samyang |
|||
Melt Flow | 25 g/10 min @Load 10.00 kg |
25 g/10 min @Load 22.05 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® WT485 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 25 g/10 min @Load 1.20 kg, Temperature 300 °C |
25 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Polyram RamTough PZ322G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238, L |
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns Process Stability TOTAL Petrochemicals Polypropylene 3764 features excellent processability and gas fade resistance.FDA. 3764 complies with all applicable FDA regulations for food contact applicat.. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | |
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
25 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
Polyram RamSter PF300G2 PBT, 10% Glass Fiber 10% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 25 g/10 min | 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 220 °C |
25 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 25 g/10 min @Load 10.0 kg, Temperature 220 °C |
25 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
ELASTO UK Dryflex® 3038-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3038-111 is specifically designe.. |
|||
Melt Flow | 25 - 35 g/10 min @Load 5.00 kg, Temperature 372 °C |
25 - 35 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Melt Flow | 25 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Fusabond® M603 Polymer Modifier Fusabond® M603 Resin is a random ethylene copolymer, incorporating a monomer which is classified as being a maleic anhydride equivalent for application uses.Fusabond® M603 is used in a variety of .. |