Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 30-2000 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® GI-2024-A LLDPE Masterbatch Resin Molded Plaque Properties. Features: Granular; improved dispersion, easy processing, good ESCR.Applications: additives, masterbatches/compounding, housewares, trashcans, containers, toys.Data provid.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Melt Flow | 20 g/10 min | 20 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Kotec Carbotex K-20UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household app.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 200 °C |
20 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kraton® D0243 K (SBS) Diblock Copolymer Kraton D0243 K is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from North America in the physical form identified:Kraton D0243 KT - sup.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 280 °C |
20 g/10 min @Load 11.0 lb, Temperature 536 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Melt Flow | >= 20 g/10 min @Load 10.0 kg, Temperature 220 °C |
>= 20 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Absolac® 150 ABS High rigidityInformation provided by Styrolution |
|||
Melt Flow | 20 g/10 min @Load 10.0 kg, Temperature 250 °C |
20 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Techmer ES HiFill® HDPE Availability: North AmericaForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RF926MO Polypropylene, Transparent Random Copolymer RF926MO is a specially modified transparent polypropylene random copolymer with high melt flow. This grade is intended for injection stretch blow molding (ISBM). and is designed for high-speed injec.. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Ivory 90034/4 Concentrate Based In LDPE DescriptionPOLYBATCH® 90034/4 is an ivory color concentrate containing based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 90034/4.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE DescriptionPOLYBATCH® 20232U is a yellow color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability .. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Yellow 2946ST Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2946ST is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2946ST co.. |
|||
Melt Flow | 20 g/10 min @Temperature 230 °C |
20 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo Pelprene™ P-70B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Blue LL40434 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL40434 is a blue concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL40434 is heavy metal fre.. |
|||
Melt Flow | 20 g/10 min | 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 20 g/10 min | 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3012E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3012E is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3012E is he.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Yellow 2214E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2214E is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2214E is h.. |
|||
Melt Flow | 20 g/10 min | 20 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP851 High Flow, Injection Molding Grade DescriptionCP 851 is a high flow injection molding grade of conventional (high pressure) low density polyethylene. ApplicationCP 851 meets the specifications in FDA Regulation 21 CFR177.1520 (c)3.1.. |
|||
Melt Flow | 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 6101RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 250 °C |
20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy Non Halogen Flame Retardant, High FlowInformation provided by E-Polymers Co. Ltd. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 2340 P Polypropylene Grade with nucleating agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition G; ASTM D1238 |
Global S-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Melt Flow | 20 g/10 min | 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 1329 UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329HU is a high flow UV stabilized, medium impact copolymer polypropylene. Information provided by A. Schulman. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |