Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 150 g/10 min @Load 1.00 kg, Temperature 235 °C |
150 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 0150 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Melt Flow | 150 - 200 g/10 min @Load 2.16 kg, Temperature 170 °C |
150 - 200 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be adde.. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | modified; ASTM D1238, ISO 1133 |
DuPont Elvax® 4320 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, s.. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-752 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | Exxon Method |
ExxonMobil Escorene® UL-7720 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | GB/T 3682-2000 |
Sichuan Deyang Haton® hd Polyphenylene Sulfide Resin Film gradeInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 230 °C |
150 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Silon Tabond 5008 Adhesive Resin Tabond 5008 is a chemically modified Polypropylene copolymer. Its functional groups improve considerably the bonding between polar polymers, metals and glass.Characteristics: • Strong adhesion .. |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 220W Ethylene Vinyl Acetate DuPont™ Elvax® 220W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 420 Ethylene Vinyl Acetate DuPont™ Elvax® 420 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 420 resins can be used for the following applications: adhesives, sealants.. |
|||
Melt Flow | >= 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
>= 150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram Bondyram® 1004 Maleic Anhydride Modified Homo-Polypropylene Recommended for coupling of wood in polypropylene composites.Information provided by Polyram. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | ASTM D1238 |
Polyram Bondyram® 1101 Maleic Anhydride Modified Homo Propylene Information provided by Polyram. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 15028CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 15028EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen.. |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesiv.. |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 7720 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7720 is a high flow, 27.6% VA copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot .. |
|||
Melt Flow | 150 g/10 min | 150 g/10 min | ASTM D1238 |
ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade) Product Description: LD 655 is a very high flow LDPE grade with a very good flexibility. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabiliz.. |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg |
150 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 6.5. |
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili.. |
|||
Melt Flow | 150 - 210 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 - 210 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group Orevac® 9305 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Hot melt adhesivesInformation provided by Arkema Group |
|||
Melt Flow | 150 g/10 min @Load 2.16 kg, Temperature 190 °C |
150 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem Evateno® HM 150 EVA Hot Melt Copolymer Evateno® HM 150 is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content, very low molecular weight, and easy crosslinkability. Evateno® HM-150 offers good compatibility wi.. |
|||
Melt Flow | 150 g/10 min @Load 5.00 kg, Temperature 275 °C |
150 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Melt Flow | 150 g/10 min @Load 10.0 kg, Temperature 360 °C |
150 g/10 min @Load 22.0 lb, Temperature 680 °F |
ISO 1133 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Melt Flow | 150 - 200 g/10 min @Load 2.16 kg, Temperature 170 °C |
150 - 200 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® 539 Thermoplastic Polyurethane Pearlbond® 539 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl.. |