Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 100 - 150 g/10 min @Load 2.16 kg, Temperature 170 °C |
100 - 150 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | ASTM D1238 |
Flint Hills AP5995-HA Polypropylene Impact Copolymer Features: Nucleated with slip, fast cycle times, high flowability.Applications: Injection Molding: High speed packaging applications and thin wall containersInformation Provided by Flint Hills Resou.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | ASTM D1238 |
Hyosung Topilene HJ145 PP HJ145 High Isostatic PP Impact CopolymerApplications:Low pressure injection moldingAutomobile partsCharacteristics:High flowabilityHigh stiffnessMedium impactInformation provided by Hyosung Corporat.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) EP-N31MA Polypropylene EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furnitu.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Pro-faxâ„¢ SC973 Polypropylene Copolymer Description: Pro-faxâ„¢ Ultra SC973 fully formulated (antistatic, nucleated, slip modified), very high melt flow, impact polypropylene reactor copolymer resin is designed for injection molding ap.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL HF5150H PP+MF15%, High Flow Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 3541 Clear TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 316 °C |
100 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 316 °C |
100 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 316 °C |
100 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® QC200N Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 316 °C |
100 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® QC200P Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 190 °C |
100 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex TEKBOND® 6700-35 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 190 °C |
100 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Polyram BondyRam® 1001 Maleic Anhydride modified Homo-polypropylene coupling agent Maleic Anhydride modified Homo-polypropylene recommended for coupling of glass and other fillers in polypropylene compositesInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 100 g/10 min @Load 2.13 kg, Temperature 190 °C |
100 g/10 min @Load 4.70 lb, Temperature 374 °F |
ISO 1133 |
Polyram Bondyram® 1001CN Maleic Anhydride Modified Co-Polymer Propylene Recommended for coupling of glass and other fillers in polypropylene composites.Information provided by Polyram. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | ASTM D1238, L |
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applicat.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | ASTM D1238L |
Total PPH 3860X Polypropylene, Extrusion Grade High flow reactor grade homopolymer for nonwoven fibersHigh Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.FDA - FINA 3860X complies with all applicable FDA.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 13442 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 13442 is a nucleated antistatic heterophasic copolymer. PPC 13442 is characterized by very high fluidity with good mechanical properties. It has been formulated for excellent ant.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 13812 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 13812 is a high fluidity heterophasic copolymer resin with fast nucleation.Polypropylene PPC 13812 is characterized by good stiffness and impact resistance as well as low shrinkage.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 260 °C |
100 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 260 °C |
100 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® CF 7 PA* Product description Grilon CF 7 is a Copolyamide. Good flexibility and toughnessGood thermoforming and orientation propertiesGood shrink characteristicsGood transparencyReduced melting point Grilon .. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP7905E1 Polypropylene Homopolymer Product Description: A high crystallinity, low impact strength copolymer resin designed for compounding base or injection molding applications requiring very high melt flow rate.Availability: North.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® BM 17 PA* Product description: Grilon BM 17 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 17 natural has the following features: High flexibility and toughnessVery good ori.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI41000WM Impact Copolymer Polypropylene Description: High flexural modulus, excellent mold release, antistatic.Applications: Suggested uses include intricately designed parts, thin-walled parts, dairy containers.Process: Injection Molding.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 275 °C |
100 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Melt Flow | 100 g/10 min @Load 5.00 kg, Temperature 275 °C |
100 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper.. |
|||
Melt Flow | 100 g/10 min @Load 2.16 kg, Temperature 230 °C |
100 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
BP Amoco Accpro® 9965 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® BM 16 nat PA* Product description: Grilon BM 16 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 16 natural has the following features: High flexibility and toughnessVery good ori.. |
|||
Melt Flow | 100 g/10 min | 100 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® G 16 PA6I/6T Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of co.. |