Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY FXW750SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Med. Heat & Impact Resin |
|||
Melt Flow | 10.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
Melt Flow | 10.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXM941A PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Melt Flow | 10.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon TA 2322 HD Blue Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2322 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |
|||
Melt Flow | 10.2 g/10 min | 10.2 g/10 min | ASTM D1238, L |
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stabilityProcess Stability. 3662 features excellent processability and the good.. |
|||
Melt Flow | 10.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1080 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets, medical.ISO data provided by the manufacturer, Arkema. |