Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | ASTM D1238 |
Plaskolite West Optix® CA-945 Clear Impact Modified Acrylic Resin Impact modified acrylic resin, extrusion and injection moldingApplications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times .. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
Compression Molded; ASTM D1238 |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg |
1.7 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Reclair F22020 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 1830E Polyethylene
(discontinued **) Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 800A Polyethylene
(discontinued **) Polyethylene 800A is a general-purpose low density formulation used for injection molding applications that require good stress-crack resistance. Polyethylene 800E is used in general-purpose extrus.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6838-862A Polyethylene
(discontinued **) E6838-862A is a low density formulation suggested for injection molding applications, such as closuresInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemic.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | melt index; ASTM D1238 |
Asahi Kasei Tenac® 2013A Acetal Homopolymer, UV Stabilized
(discontinued **) Similar to 3013A, but higher in molecular weight.Applications: Pipe fittings, rollers, exterior automotive parts.This product is not a part of the standard product line dated 2003. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
Compression Molded; ASTM D1238 |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | ASTM D1238 |
LyondellBasell Plexar® PX3227 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Global GP-110 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H01H-00 Polypropylene Homopolymer This is a low flow rate homopolymer designed for extrusion or injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applic.. |
|||
Melt Flow | 1.7 - 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 - 2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem LB 0216 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
IRPC Polimaxx Polene GP110 Polystyrene APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | ISO 1133 |
Lucite International Diakon® CLH952L Acrylic Polymer Information provided by Lucite International |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | ASTM D1238/E |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN®-V 420 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EM800AA Low Density Polyethylene WESTLAKE low-density polyethylene EM800 is a general-purpose low-density formulation used for injection molding applications that require good stress-crack resistance.Application/UsesCosmetics/perso.. |
|||
Melt Flow | 1.7 g/10 min | 1.7 g/10 min | 190 / 21.6 (HLMI); ASTM D1238 |
ExxonMobil Paxon™ FD60-018 Compression Molding Resin FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti.. |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 6502 MR Natural TPE Thermoplastic Elastomer Forms: PelletsInformation provided by Multibase |