Apparent Bulk Density 0.850 - 1.00 g/cc
0.0307 - 0.0361 lb/in³
ISO 60
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Apparent Bulk Density 0.850 - 1.00 g/cc
0.0307 - 0.0361 lb/in³
ISO 60
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
Apparent Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
ISO 60
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Apparent Bulk Density 0.700 - 1.00 g/cc
0.0253 - 0.0361 lb/in³
ISO 60
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
Apparent Bulk Density 0.700 - 1.00 g/cc
0.0253 - 0.0361 lb/in³
ISO 60
Raschig Group EPOXIDUR® 3582 EP Epoxy
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi..
Apparent Bulk Density 0.700 - 1.00 g/cc
0.0253 - 0.0361 lb/in³
ISO 60
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Apparent Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Apparent Bulk Density 0.750 - 1.00 g/cc
0.0271 - 0.0361 lb/in³
ISO 60
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Copyright © lookpolymers.com All Rights Reserved