Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Apparent Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ASTM D1895 |
Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Apparent Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Apparent Bulk Density | 0.730 - 0.850 g/cc | 0.0264 - 0.0307 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Apparent Bulk Density | 0.730 g/cc | 0.0264 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |