Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f.. |
|||
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | ISO 60 |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | Apparent density per ASTM D1895 |
Plenco 7300 Phenolic, Nodular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |
|||
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | Apparent density per ASTM D1895 |
Plenco 7466 Phenolic, Granular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406.. |
|||
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | ASTM D1895 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | TRM-37 |
Tipco Tipcolite® THD 311 Phenolic Compound, Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Apparent Bulk Density | 0.620 - 0.680 g/cc | 0.0224 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Apparent Bulk Density | 0.620 - 0.700 g/cc | 0.0224 - 0.0253 lb/in³ | IS 867-1963 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Apparent Bulk Density | 0.620 - 0.690 g/cc | 0.0224 - 0.0249 lb/in³ | IS 867-1963 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Apparent Bulk Density | 0.620 - 0.680 g/cc | 0.0224 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Apparent Bulk Density | 0.620 - 0.700 g/cc | 0.0224 - 0.0253 lb/in³ | IS 867-1963 |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Apparent Bulk Density | 0.620 - 0.680 g/cc | 0.0224 - 0.0246 lb/in³ | IS 867-1963 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Apparent Bulk Density | 0.620 g/cc | 0.0224 lb/in³ | ASTM D1895 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound