Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 1.00 - 1.30 g/cc | 0.0361 - 0.0470 lb/in³ | ISO 60 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Apparent Bulk Density | 1.00 - 1.30 g/cc | 0.0361 - 0.0470 lb/in³ | ISO 60 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Apparent Bulk Density | 0.930 - 1.30 g/cc | 0.0336 - 0.0470 lb/in³ | Average value: 1.06 g/cc Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
Apparent Bulk Density | 0.700 - 1.30 g/cc | 0.0253 - 0.0470 lb/in³ | Average value: 0.950 g/cc Grade Count:5 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |