Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.850 - 1.00 g/cc | 0.0307 - 0.0361 lb/in³ | ISO 60 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Apparent Bulk Density | 0.850 - 1.00 g/cc | 0.0307 - 0.0361 lb/in³ | ISO 60 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Apparent Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | ISO 60 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Apparent Bulk Density | 0.700 - 1.00 g/cc | 0.0253 - 0.0361 lb/in³ | ISO 60 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Apparent Bulk Density | 0.700 - 1.00 g/cc | 0.0253 - 0.0361 lb/in³ | ISO 60 |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Apparent Bulk Density | 0.700 - 1.00 g/cc | 0.0253 - 0.0361 lb/in³ | ISO 60 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Apparent Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Apparent Bulk Density | 0.750 - 1.00 g/cc | 0.0271 - 0.0361 lb/in³ | ISO 60 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |