Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.540 - 0.780 g/cc | 0.0195 - 0.0282 lb/in³ | Average value: 0.618 g/cc Grade Count:5 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Apparent Bulk Density | 0.550 - 0.780 g/cc | 0.0199 - 0.0282 lb/in³ | Average value: 0.650 g/cc Grade Count:5 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Apparent Bulk Density | 0.680 - 0.780 g/cc | 0.0246 - 0.0282 lb/in³ | IS 867-1963 |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Apparent Bulk Density | 0.470 - 0.780 g/cc | 0.0170 - 0.0282 lb/in³ | Average value: 0.549 g/cc Grade Count:11 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |