Physical Properties Metric English Comments
Apparent Bulk Density 0.470 g/cc
0.0170 lb/in³
NanoAmor 95%, OD/WT/L: 20-40/5-15 nm/0.5-5 um Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Apparent Bulk Density 0.470 - 0.620 g/cc
0.0170 - 0.0224 lb/in³
Average value: 0.551 g/cc Grade Count:9
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Apparent Bulk Density 0.470 - 0.470 g/cc
0.0170 - 0.0170 lb/in³
ASTM D792
LyondellBasell Montell 1900 UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp..
Apparent Bulk Density 0.470 - 0.470 g/cc
0.0170 - 0.0170 lb/in³
ASTM D792
LyondellBasell Montell 1900CM UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, ..
Apparent Bulk Density 0.470 - 0.470 g/cc
0.0170 - 0.0170 lb/in³
ASTM D792
LyondellBasell Montell 1900H UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, ..
Apparent Bulk Density 0.470 - 0.470 g/cc
0.0170 - 0.0170 lb/in³
ASTM D792
LyondellBasell Montell 1900LCM UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp..
Apparent Bulk Density 0.470 g/cc
0.0170 lb/in³
ISO 60
SolVin 271DF Polyvinyl Chloride General Purpose - Plasticized
Made by suspension polymerization. APPLICATIONS Extrusion : - plasticized and semi-rigid profiles and pipes - blowing of plasticized films Calendering : opaque or transparent, plasticized and semi-r..
Apparent Bulk Density 0.470 - 0.530 g/cc
0.0170 - 0.0191 lb/in³
ISO 60:1977
BorsodChem ONGROVIL S-494 Suspension PVC-Resin
S-494 is a suspension type PVC homopolymer of high molecular mass. It is characterized by a porous particle structure and a narrow range of particle size. It retains its excellent pourability even a..
Apparent Bulk Density 0.470 - 0.530 g/cc
0.0170 - 0.0191 lb/in³
ISO 60:1977
BorsodChem ONGROVIL S-5070 Suspension PVC-Resin
S-5070 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r..
Apparent Bulk Density 0.470 - 0.780 g/cc
0.0170 - 0.0282 lb/in³
Average value: 0.549 g/cc Grade Count:11
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Apparent Bulk Density 0.470 g/cc
0.0170 lb/in³
ISO 60
SolVin 275SC Polyvinyl Chloride General Purpose - Plasticized
Made by suspension polymerization. APPLICATIONS Extrusion : - plasticized and semi-rigid profiles and pipes Calendering : opaque or transparent, plasticized and semi-rigid films and sheets.Informati..