Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3500 - 5000 cP | 3500 - 5000 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | |
Huntsman Araldite GY 508 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 390 to 425. Max color is 5.Comments/Applications: BPA epoxy blended with a polyglycol di-epoxide. The higher EEW allows much lower hardener levels. Flexible resin f.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | |
Huntsman HY 943 Aliphatic Amine Approx. H+ equivalent weight 38. Mix Ratio with GY 6010 is 20.Comments/Applications: Aliphatic amine adduct, light colored, very reactive. Coatings with excellent resistance to organic solvents a.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | |
Huntsman Kerimid 8292 N-75 Resin Comments/Applications: Kerimid 8292 supplies as a 75% by weight solution in MEK.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | |
Huntsman MY 0500 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 105 to 115. Max color is 11.Comments/Applications: Trifunctional low viscosity epoxy resin based on para amino phenol. Performance upgrader for bisphenol A resins. .. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1101 A (SBS) Liner Block Copolymer Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | 25% Toluene Solution; KM 06 |
Kraton® D1101 E (SBS) Liner Block Copolymer Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Viscosity | 3000 - 5000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3000 - 5000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2091104D1 Conductive Silver Adhesive This ink can be used in a wide range of applications, as a conductive adhesive, it has excellent chemical resistance, with good adhesion. This product is based on a unique curing process that resul.. |
|||
Viscosity | 3500 - 5000 cP | 3500 - 5000 cP | |
Lucite International Colacryl ® 1204 Acrylic Solution Resin Butyl Methacrylate polymers are more flexible and softer than Methyl Methacrylate types. The polymers are compatible with nitrocellulose, chlorinated rubber, some phenolics and maleics. Butyl methac.. |
|||
Viscosity | 2500 - 5000 cP @Temperature 25.0 °C |
2500 - 5000 cP @Temperature 77.0 °F |
|
Lucite International Colacryl ® TS1778 Acrylic Solution Resin Colacryl TS 1778 is a self cross-linking acrylic copolymer designed for adhesive applications. Once dried, a film cast from this product remains permanently tacky.Suggested Uses: Pressure-sensitiv.. |
|||
Viscosity | 3600 - 5000 cP | 3600 - 5000 cP | |
Huntsman MY 721 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 109 to 117. Color: BrownComments/Applications: Lowest viscosity, tetra-functional epoxy with the same chemistry as MY 720. Used for high performance composites, adhe.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A7810L TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A8510L TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | 20% Viscosity, 1-2% NaCl |
Solvay MACKADET® DR-100M Surfactant Product Description: Mackadet® DR-100M is a concentrated blend of surfactants, which simply requires dilution and the addition of minor additives to produce a ready to package high foaming produc.. |
|||
Viscosity | 1000 - 5000 cP | 1000 - 5000 cP | #3 Spindle, 12 rpm >1 min; RP-17619 |
Solvay MIRACARE® SLB-365/N Surfactant Description: Surfactant blend used in the production of structured liquid formulations. The preservative in MIRACARE SLB-365/N is a non-formaldehyde donor (Neolone).I.N.C.I. Name: WATER, SODIUM TRID.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | Part B |
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive .. |
|||
Viscosity | 200 - 5000 cP | 200 - 5000 cP | Unmilled Cement; Zeon Test #1377 |
Zeon Chemicals Nipol® 1072 Carboxylated Nitrile Elastomer Nipol 1072 is a copolymer of butadiene and acrylonitrile with medium oil resistance, modified to contain free carboxylic groups. Sufficient non-staining antioxidant is added during manufacture for n.. |
|||
Viscosity | 2500 - 5000 cP | 2500 - 5000 cP | Part B |
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1051 Nitrile Elastomer Nipol 1051 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Easy processing version of Ni.. |
|||
Viscosity | 1200 - 5000 cP | 1200 - 5000 cP | Thixotropic |
Loctite® 222 Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 1800 - 5000 cP | 1800 - 5000 cP | Thixotropic |
Loctite® 262 Medium to High Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 800 - 5000 cP | 800 - 5000 cP | Dynamic |
Dow Corning XIAMETER® PMCPOFX-8040 Fluid Is chemically equivalent to DOW CORNING® 2-8040 POLYMER. Diaminofunctional silicone softener; suitable for formulation to a microemulsion that can be applied to all types of woven or knitted fabric.. |
|||
Viscosity | 3500 - 5000 cP @Temperature 23.0 °C |
3500 - 5000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
Viscosity | 3000 - 5000 cP @Temperature 23.0 °C |
3000 - 5000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Viscosity | 3000 - 5000 cP @Temperature 23.0 °C |
3000 - 5000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 375 High Temperature Epoxy Product Description: EPO-TEK®375 is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. Also available in a single component frozen sy.. |
|||
Viscosity | 3000 - 5000 cP | 3000 - 5000 cP | |
Epoxyset Epoxibond EB-119SP Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Viscosity | 4000 - 5000 cP | 4000 - 5000 cP | |
Epoxyset Epoxiohm EO-23M Electrically Conductive Epoxy Adhesive EO-23M is an electrically conductive, low viscosity silver-filled epoxy adhesive. Used for hybrid / micro-electronic adhesive including die-attach and substrate attach for Rf and Microwave devices.I.. |
|||
Viscosity | 4200 - 5000 cP @Temperature 35.0 °C |
4200 - 5000 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G211 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | |
Beijing Ranger Chem SM-634X85 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 4200 - 5000 cP @Temperature 35.0 °C |
4200 - 5000 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G222 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |