Polymer Property : Viscosity = 1500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1000 - 1500 cP
1000 - 1500 cP
ND Industries 331 Surface Insensitive Instant Superglue
Medium-high viscosity for difficult to bond surfaces
Viscosity 1200 - 1500 cP
1200 - 1500 cP
Thixotropic
ND Industries NutGrade® 121 Removable Threadlocker
A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th..
Viscosity 1200 - 1500 cP
1200 - 1500 cP
Thixotropic
ND Industries ScrewGrade® 111 Removable Threadlocker
A low strength threadlocker which eliminates vibrational loosening, and seals against leakage and corrosion.Typical Usessoft metal fasteners, precision screws, and locking fasteners smaller than .25..
Viscosity 1000 - 1500 cP
1000 - 1500 cP
ND Industries SuperGlue Ethyl 316
Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III
Viscosity 800 - 1500 cP

@Temperature 23.9 °C
800 - 1500 cP

@Temperature 75.0 °F
TSE Industries EcoWIND® 200 Polyurethane Resin Filament Winding  (discontinued **)
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Viscosity 900 - 1500 cP
900 - 1500 cP
Huntsman Araldite ECN 1400 Water-Based Adhesive/Coating
Base Resin is ECN 1299. Typical Solids Content 40%. Mean Particle Size 4µm. Weight per Epoxide (EEW, g/eq), solids basis, 220 to 250.Comments/Applications: Adhesives; Fiber-Sizing; Textiles; A..
Viscosity 900 - 1500 cP
900 - 1500 cP
20% Toluene Solution at 25°C; BAM 922
Kraton® G1660 H (SEBS) Linear Triblock Copolymer
Description: Kraton G1660 H is a linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 31%. It is supplied from North America in the physical form identified..
Viscosity 1000 - 1500 cP

@Temperature 20.0 °C
1000 - 1500 cP

@Temperature 68.0 °F
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup
Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International
Viscosity 1000 - 1500 cP
1000 - 1500 cP
Huntsman Tactix 556 Epoxy
Weight per Epoxide (EEW, g/eq) 215 to 235.Comments/Applications: Dicyclopentadiene based epoxy. Very low moisture pickup. Suggested for adhesives and composites used at elevated temperatures in a ..
Viscosity 1000 - 1500 cP
1000 - 1500 cP
Huntsman Tactix 556 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 215 to 235.Comments/Applications: Dicyclopentadiene based epoxy. Very low moisture pickup. Suggested for adhesives and composites used at elevated temperatures in a ..
Viscosity 900 - 1500 cP
900 - 1500 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1102 A (SBS) Liner Block Copolymer
Description: Kraton D1102 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Viscosity 500 - 1500 cP
500 - 1500 cP
RP-0596
Solvay ALCOCARE® 6012 Surfactant
Description: NSF Registered product accepted for use as a hand washing and sanitizing compound (E-2 Rated Cleanser) for use in and around food processing areas. Sub-registration is required.Chemical..
Viscosity 1200 - 1500 cP

@Temperature 23.0 °C
1200 - 1500 cP

@Temperature 73.4 °F
Master Bond UV10MED Biocompatible One Component UV Curable Adhesive System
Master Bond UV10Med is a one part UV type system for bonding, sealing and coating. It fully passes USP Class VI testing requirements and features good optical clarity and physical properties as well..
Viscosity 100 - 1500 cP
100 - 1500 cP
Milled Cement; Zeon Test #1377
Zeon Chemicals Nipol® 1472X Nitrile Powder and Crumb Elastomer
Nipol 1472X is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile contnet modified to contain carboxyl groups. It contains sufficient antioxidant for normal storage conditions. ..
Viscosity 1200 - 1500 cP

@Temperature 23.9 °C
1200 - 1500 cP

@Temperature 75.0 °F
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Viscosity 1000 - 1500 cP

@Temperature 23.0 °C
1000 - 1500 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy
Material Description: A single component, UV curable, thixotropic flexible epoxy adhesive/encapsulant designed for semiconductor and opto-electronic packaging. Glob top over IC and wire bonds, and ..
Viscosity 1100 - 1500 cP
1100 - 1500 cP
Aremco Aremco-Seal™ 617 High Temperature Glass Coating
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC).
Viscosity 1100 - 1500 cP
1100 - 1500 cP
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass
Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors.
Viscosity 100 - 1500 cP
100 - 1500 cP
Beijing Ranger Chem SM-601REK70 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 500 - 1500 cP
500 - 1500 cP
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating
This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f..
Viscosity 1200 - 1500 cP

@Temperature 23.9 °C
1200 - 1500 cP

@Temperature 75.0 °F
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Viscosity 800 - 1500 cP

@Temperature 23.0 °C
800 - 1500 cP

@Temperature 73.4 °F
Master Bond UV15-7SP4DC One Component, Dual Cured, Flexible UV System
Master Bond Polymer System UV15-7SP4DC is a one component, optically clear, dual cured flexible UV and/or heat curable polymer system with extended service capability of -80°F to +250°F. It cures ..
Viscosity 500 - 1500 cP

@Temperature 20.0 °C
500 - 1500 cP

@Temperature 68.0 °F
15% solution in MEK; MQSA 40 A
Lubrizol Advanced Materials Disperbond® D31S Thermoplastic Polyurethane  (discontinued **)
Disperbond® originates from a new Merquinsa proprietary technology that produces linear, aromatic thermoplastic polyurethanes in pellet form. These TPUs can be dissolved in acetone. In a further ..
Viscosity 1300 - 1500 cP

@Temperature 60.0 °C
1300 - 1500 cP

@Temperature 140 °F
C.O.I.M. DIEXTER® G235 Polyol Polyester
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt..
Viscosity 100 - 1500 cP
100 - 1500 cP
Unmilled Cement; Zeon Test #1377
Zeon Chemicals Nipol® 1072CGX Carboxylated Nitrile Elastomer
Nipol 1072CGX is a copolymer of butadiene and acrylonitrile with medium oil resistance modified to contian free carboxylic groups and is soluble in MEK without mill brakdown. Sufficient antioxidant ..
Viscosity 900 - 1500 cP

@Temperature 25.0 °C
900 - 1500 cP

@Temperature 77.0 °F
Uncured
Permabond 947 Cyanoacrylate, low odor
PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad..