Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 800000 cP @Shear Rate 250 1/s, Temperature 230 °C |
800000 cP @Shear Rate 250 1/s, Temperature 446 °F |
|
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The .. |
|||
Viscosity | 800000 cP | 800000 cP | melt; SABIC Method |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Viscosity | 800000 cP @Temperature 420 °C |
800000 cP @Temperature 788 °F |
melt; ISO 11443 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Viscosity | 800000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
800000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Viscosity | 800000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
800000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Viscosity | 800000 cP @Shear Rate 25.0 1/s, Temperature 320 °C |
800000 cP @Shear Rate 25.0 1/s, Temperature 608 °F |
|
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
(discontinued **) Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui.. |
|||
Viscosity | 800000 cP | 800000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2090-30AB Elastomer KE-2090-30 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 800000 cP | 800000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 800000 cP | 800000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2090-50AB Elastomer KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 800000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
800000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Viscosity | 800000 - 3.75e+6 cP | 800000 - 3.75e+6 cP | Thixotropic |
Loctite® Gasket Eliminator® 518 Flange Sealant Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can.. |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F130-E5 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F132-E2 PA6 High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 800000 cP @Temperature 160 °C |
800000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 800000 cP @Temperature 160 °C |
800000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 800000 cP @Temperature 160 °C |
800000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 800000 cP @Shear Rate 0.100 1/s, Temperature 240 °C |
800000 cP @Shear Rate 0.100 1/s, Temperature 464 °F |
|
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 800000 - 1.20e+6 cP | 800000 - 1.20e+6 cP | |
BASF Master Builders Solutions ChemRex® CX-948 Urethane Adhesive/Sealant Typical applications include high-solids subfloor adhesive, manufacture of windows, doors, and panels, and the assembly of trucks, cabs, and vans.The working open time is 45-60 minutes. The freeze-.. |
|||
Viscosity | 800000 - 1.30e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
800000 - 1.30e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Viscosity | 800000 cP @Shear Rate 300 1/s, Temperature 190 °C |
800000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 1080 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 800000 cP | 800000 cP | Part A, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Viscosity | 800000 cP | 800000 cP | Part A, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Viscosity | 800000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
800000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |