Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 750000 - 3.75e+6 cP | 750000 - 3.75e+6 cP | |
Ritelok GM18 Aluminum Parts Gasket Maker Anaerobic. Flexible gasket maker for aluminum flanges. Replaces pre-cut gaskets, Does not shrink or relax, flexible, Withstands temperatures from 65°F to 300°F (55°C)-150°C), .. |
|||
Viscosity | 750000 cP | 750000 cP | Before Sintering |
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual package.. |
|||
Viscosity | 750000 cP | 750000 cP | RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Viscosity | 750000 cP | 750000 cP | RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem.. |
|||
Viscosity | 750000 cP | 750000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 750000 cP | 750000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 750000 cP | 750000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Viscosity | 750000 cP | 750000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Viscosity | 750000 cP @Temperature 160 °C |
750000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 8E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 750000 cP @Shear Rate 100 1/s, Temperature 175 °C |
750000 cP @Shear Rate 100 1/s, Temperature 347 °F |
Dow Method |
Dow XU 32019.10 Barrier Polymer Excellent oxygen and water vapor barrier Information provided by Dow |
|||
Viscosity | 750000 cP | 750000 cP | Mixed; TM R050-12 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |