Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 600 - 900 cP @Temperature 25.0 °C |
600 - 900 cP @Temperature 77.0 °F |
|
Northstar Polymers PLA-012 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 cP @Temperature 25.0 °C |
600 cP @Temperature 77.0 °F |
|
Northstar Polymers PNA-157 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 - 1200 cP @Temperature 25.0 °C |
600 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers PNC-153 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 cP | 600 cP | |
Resinlab® RC8040 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Viscosity | 600 - 1200 cP @Temperature 71.1 °C |
600 - 1200 cP @Temperature 160 °F |
|
Northstar Polymers PAA-109 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 600 - 4200 cP @Temperature 140 - 140 °C |
600 - 4200 cP @Temperature 284 - 284 °F |
Average value: 1.60e+6 cP Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 600 cP @Temperature 30.0 °C |
600 cP @Temperature 86.0 °F |
|
DSM Somos® 8120 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Viscosity | 600 - 1200 cP | 600 - 1200 cP | |
Huntsman Araldite EPN 1138 MAK-80 Epoxy Phenol Novolac Weight per Epoxide (EEW, g/eq) 175 to 181. Max color is 2.Comments/Applications: EPN 1138 80% solids in Methyl n-Amyl Ketone. High performance, chemically resistant tank linings, maintenance coati.. |
|||
Viscosity | 600 - 1300 cP | 600 - 1300 cP | |
Huntsman AroCy M-30 Bisphenol Dicyanate Prepolymer Comments/Applications: Improved hot wet performance. Used primarily in the manufacture of prepreg for structural composites and tooling. High temperature adhesive.Data provided by Ciba Specialty C.. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | |
Huntsman AroCy XU 378 Cyanate Ester Comments/Applications: Novolac cyanate ester. High temperature composites and adhesives, where a Tg greater than 300°C is required.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemic.. |
|||
Viscosity | 600 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
600 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
Apparent melt viscosity; ASTM D3835 |
Metabolix M-veraâ„¢ B5008 Film Grade Compostable Bioplastic B5008 is a compostable film product with 30% biobased carbon content that is ideal for compost bags and can liners used for organic waste diversion and for shopping and retail bags.Features:Meets re.. |
|||
Viscosity | <= 600 cP @Time 60.0 sec |
<= 600 cP @Time 0.0167 hour |
#60 spindle, 60 rpm; LSY-QB-ID006 |
LG Chemical Lutex 703 SBR Latex Description: Binding Force, Ink set off, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Pre-Rod, Blade Coater, Adhesive coated paper and Carpet back-coating .. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1114 P (SIS) Linear Triblock Copolymer Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: .. |
|||
Viscosity | <= 600 cP @Temperature 25.0 °C |
<= 600 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil E5S Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Viscosity | <= 600 cP @Temperature 25.0 °C |
<= 600 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil E3 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | #3 sp @ 60 rpm; RP-0596 |
Solvay RHODOLINE® LC-2 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: DEFOAMER BLENDAvailable in: North America.. |
|||
Viscosity | 600 cP @Temperature 23.0 °C |
600 cP @Temperature 73.4 °F |
|
Master Bond EP19HT One Component, Storage Stable Epoxy System Master Bond Polymer System EP19HT is a storage stable one component liquid epoxy resin system for durable, high performance adhesive/sealants, impregnants and liners. It features excellent storage c.. |
|||
Viscosity | 600 cP @Temperature 25.0 °C |
600 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond FS227 Thixotropic Epoxy/Polyamide Adhesive TRA-BOND FS227 is a thixotropic (thick paste) polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wettin.. |
|||
Viscosity | 600 cP | 600 cP | |
Loctite® 4471 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 600 cP | 600 cP | |
Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant |
|||
Viscosity | 600 cP @Temperature 50.0 °C |
600 cP @Temperature 122 °F |
|
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Viscosity | 600 cP | 600 cP | B Side |
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim.. |
|||
Viscosity | 600 - 900 cP | 600 - 900 cP | |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Viscosity | 600 - 900 cP | 600 - 900 cP | |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |
|||
Viscosity | 600 cP | 600 cP | uncured |
Atom Adhesives AA-BOND FS227 Epoxy Adhesive AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a.. |
|||
Viscosity | 600 cP | 600 cP | B Side |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |
|||
Viscosity | 600 - 45000 cP @Temperature 165 - 175 °C |
600 - 45000 cP @Temperature 329 - 347 °F |
Average value: 6480 cP Grade Count:48 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Viscosity | 600 cP | 600 cP | |
Solvay ANTAROX® 17-R-4 Surfactant Chemical Name: EO/PO BLOCK COPOLYMERCAS: 9003-11-6, 7732-18-5Water solubility: SolubleAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX 17-R-4 is dispersible i.. |