Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1900 - 2100 cP | 1900 - 2100 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE 2000CP FLUORESCENT Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE FLUORESCENT advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performan.. |
|||
Viscosity | 1900 cP @Temperature 25.0 °C |
1900 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system .. |
|||
Viscosity | 1900 cP @Temperature 25.0 °C |
1900 cP @Temperature 77.0 °F |
Mixed (lv #4, 12 rpm) |
Tra-Con Tra-Bond 526D01 Information provided by Tra-Con Inc. |
|||
Viscosity | 1900 cP @Temperature 129 - 149 °C |
1900 cP @Temperature 264 - 300 °F |
|
Hexcel® HexPly® 8551-7 Epoxy Matrix HexPly® 8551-7 is an amine-cured, toughened epoxy resin system supplied with unidirectional graphite fibers. Typical reinforcement is continuous IM7 (intermediate modulus) graphite filaments. HexPl.. |
|||
Viscosity | 1900 - 2900 cP | 1900 - 2900 cP | Cone & Plate; ISO 3219 (93) |
Dow SPECFLEX™ NC 606 Polyol SPECFLEX™ NC 606 polyol is a co-polymer polyol especially designed for the production of High Resilience (HR) molded flexible foams. It processes well on all types of foam machinery. CAS# 00908.. |
|||
Viscosity | 1900 - 2900 cP @Temperature 35.0 °C |
1900 - 2900 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® T 400 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 1900 cP | 1900 cP | A Component; Spindle #2; speed 10 rpm; ASTM D1824 |
Aptek 6100-1A/B Epoxy Encapsulant Optoelectronic grade, water clear encapsulant for IR and visible LED discreet devices. Lower Tg versions available for display devices.Part A is dark blue. Part B is clear to pale yellow.Information.. |
|||
Viscosity | 1900 cP @Temperature 177 °C |
1900 cP @Temperature 350 °F |
Typical |
Bostik 2391 Versatile, Good Hot Tack EVA Glue Stick Bostik 2391 Versatile, Good Hot Tack EVA Glue StickVersatile packaging product. Good "hot tack." |
|||
Viscosity | 1900 cP | 1900 cP | |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Viscosity | 1900 cP | 1900 cP | Mixed - low; Resin - 1,900 cP; Hardener - 2,800 cP |
Loctite® Durabond® E-05CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |