Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 17000 cP | 17000 cP | Mixed, RVT, #6, 2.5 rpm; TM R050-12 |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Viscosity | 17000 cP @Temperature 175 °C |
17000 cP @Temperature 347 °F |
Automatic orifice Viscosity |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Viscosity | 17000 - 19000 cP | 17000 - 19000 cP | |
Huntsman MY 9663 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 115 to 135. Color: BrownComments/Applications: Narrow viscosity MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistant.. |
|||
Viscosity | 17000 cP | 17000 cP | Mixed |
Tra-Con Tra-Bond 9392 Flexible Potting Epoxy Adhesive TRA-BOND 9392 is a low viscosity, two-part polyurethane formulation recommended for potting and molding where flexibility and temperature resistance are required. TRA-BOND 9349 is a room temperature.. |
|||
Viscosity | 17000 cP | 17000 cP | at 20 RPM |
Loctite® SpeedBonder™ 324 High Impact Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 17000 cP | 17000 cP | dynamic, mixing |
Dow Corning HS IV BASE & 10:1 COLORED CATALYST High strength lowest durometer silicone mold making rubber, suited for the production of print pads and for the detailed reproduction of fiines and art objects. HS IV Base with HS IV 10:1 Colored Ca.. |
|||
Viscosity | 17000 cP | 17000 cP | |
Dymax 9-20558 Conformal Coating High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20558 Conformal CoatingThick barrier coating; excellent protection of sensitive circuits from moisture. Cure Speed.. |
|||
Viscosity | 17000 cP | 17000 cP | Base |
ACC QM 230 QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material QM 230 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Viscosity | 17000 cP | 17000 cP | Base |
ACC QM 230F QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for t.. |
|||
Viscosity | 17000 - 21000 cP | 17000 - 21000 cP | Accelerator |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Viscosity | 17000 cP | 17000 cP | |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |
|||
Viscosity | 17000 cP @Temperature 25.0 °C |
17000 cP @Temperature 77.0 °F |
|
Abatron AboCast/AboCure 8501-6/8501-4 High Temperature Resistant Epoxy 1-component system. Clear amber, low viscosity, structural/dielectric epoxy.Processing: Pot Life: 5-9 months. Cured 2 hours at 95°C + 15 hour post-cure at 230°C. Information provided by Abatron... |
|||
Viscosity | 17000 cP | 17000 cP | Mixed, RVT, #6, 2.5 rpm; TM R050-12 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Viscosity | 17000 - 50000 cP | 17000 - 50000 cP | Thixotropic |
Loctite® 572 Low Strength Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 17000 cP | 17000 cP | with hardener |
Devcon Zip Patch™ Epoxy Emergency Repair ProductsComments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-u.. |