Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 12000 - 16000 cP | 12000 - 16000 cP | |
ND Industries 440 High pressure Sealant Pneumatic and hydraulic sealant fluid, for power and gas system connections |
|||
Viscosity | 12000 - 175000 cP | 12000 - 175000 cP | |
ND Industries 907 Anti-seize Nickel-Graphite Nickel anti-seize for high temperatures and severe service |
|||
Viscosity | 12000 cP | 12000 cP | Mixed; TM R050-12 |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Viscosity | 12000 cP | 12000 cP | Mixed Viscosity |
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber Information provided by ITW Devcon |
|||
Viscosity | 12000 - 18000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
12000 - 18000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2041206P2 Gold Polymer Electrode Paste Gold paste is a screen printable gold polymer paste designed as a working electrode in electrochemical biosensors. This is used as a working electrode in medical diagnostics, environmental sensor a.. |
|||
Viscosity | 12000 - 15000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
12000 - 15000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2050106D7 Carbon Graphite Ink This Carbon Graphite Ink is designed to be used for screen printing working electrodes. This is an ink which has been optimized to give superior electrochemical performance. It gives excellent elec.. |
|||
Viscosity | 12000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
12000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 35-HR-9 TPE Product Description: StarTUFF TF 35-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Viscosity | 12000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
12000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-HR-1 TPE Product Description: StarTUFF TF 40-HR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Viscosity | 12000 - 20000 cP | 12000 - 20000 cP | Mixed system |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
Viscosity | 12000 - 15000 cP | 12000 - 15000 cP | |
Master Bond Mastersil 150 Two Part, Condensation Cured, Flexible Silicone Master Sil 150 is a 2 part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation.. |
|||
Viscosity | 12000 cP @Temperature 25.0 °C |
12000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® E-1030 One-Component Epoxy Low Stress Encapsulant Emerson & Cuming E-1030 Stycast® One-Component Epoxy Low Stress EncapsulantDesigned for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low te.. |
|||
Viscosity | 12000 cP @Temperature 25.0 °C |
12000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound TRA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compon.. |
|||
Viscosity | 12000 cP | 12000 cP | Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2 |
Formosa Plastics Formolon® 38 PVC PVC Homopolymer Dispersion Resin F-38 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities, exceptional air release as well as a balance of other properti.. |
|||
Viscosity | 12000 - 15000 cP | 12000 - 15000 cP | Dynamic |
Dow Corning XIAMETER® PMCPOHX-4040 Polymer 14000CS Is chemically equivalent to DOW CORNING® 3-0084 POLYMER. Polydimethylsiloxane polymer with terminated, curable silanol functionality.Information provided by Dow Corning |
|||
Viscosity | 12000 - 20000 cP @Temperature 23.0 °C |
12000 - 20000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Viscosity | 12000 - 20000 cP @Temperature 23.0 °C |
12000 - 20000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, .. |
|||
Viscosity | 12000 - 16000 cP @Temperature 23.0 °C |
12000 - 16000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope.. |
|||
Viscosity | 12000 cP @Temperature -40.0 °C |
12000 cP @Temperature -40.0 °F |
|
ConocoPhillips Hydroclear® V Automatic Transmission Fluid Description: Conoco Hydroclear MERCON V Automatic Transmission Fluid is a premium multifunctional product that has been approved for use in all General Motors and Ford transmissions. It carries both.. |
|||
Viscosity | 12000 cP | 12000 cP | |
ACC MM828 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 12000 - 14000 cP | 12000 - 14000 cP | |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Viscosity | 12000 cP | 12000 cP | mixed |
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina Coarse grain castable for producing large hi-temp tooling. |
|||
Viscosity | 12000 cP | 12000 cP | mix |
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide Single-part castable ceramic exhibiting high strength and thermal conductivity. |
|||
Viscosity | 12000 - 15000 cP | 12000 - 15000 cP | |
Beijing Ranger Chem SM-828CA Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 12000 cP | 12000 cP | |
3M Scotch-Weld™ DP270 Clear Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Viscosity | 12000 cP | 12000 cP | catalyzed with QM CAT RED 3 |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 12000 cP | 12000 cP | catalyzed with QM CAT PURPLE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 12000 cP @Temperature -40.0 °C |
12000 cP @Temperature -40.0 °F |
|
ExxonMobil Mobil Multi-Vehicle ATF Mobil Multi-Vehicle ATF is a premium synthetic blend lubricant formulated to provide excellent service in a wide variety of automotive automatic transmission applications. It is approved for use i.. |