Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.0400 - 6000 cP | 0.0400 - 6000 cP | Average value: 1190 cP Grade Count:51 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 2500 - 6000 cP | 2500 - 6000 cP | |
Huntsman Araldite GZ 571 KX-75 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 450 to 530. Max color is 3.Comments/Applications: GT 7071 - 75% solids in MIBK (16%) and xylene (9%). High performance 2-package system for coatings, flooring and ge.. |
|||
Viscosity | 3000 - 6000 cP | 3000 - 6000 cP | |
Huntsman Araldite GZ 7488 V-40 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 6600 to 10000. Max color is 4.Comments/Applications: Very high molecular weight epoxy resin, 40% solids in PM acetate. Outstanding adhesion, excellent flexibility an.. |
|||
Viscosity | 3000 - 6000 cP | 3000 - 6000 cP | |
Huntsman HY 840 US Polyamide Approx. H+ equivalent weight 130. Mix Ratio with GY 6010 is 81.Comments/Applications: Solvent free, low viscosity, high amine content with higher flexibility and toughness. Flexible mix ratio 33 .. |
|||
Viscosity | 3000 - 6000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
3000 - 6000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink UV curable Silver conductor ink specifically designed for printing on to polymeric substrates using flexographic printing. Ink can be printed at speeds up to 13m/min, with good line definition and .. |
|||
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A7710 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Viscosity | 1000 - 6000 cP | 1000 - 6000 cP | LVT SP #3, 12 rpm; RP-17619 |
Solvay MIRACARE® SLB-205/N Surfactant Description: Miracare SLB-205/N is a free flowing, high active surfactant concentrate used in the preparation of structured liquids. It is a surfactant base used to stabilize additives applied in a .. |
|||
Viscosity | 5000 - 6000 cP @Temperature 23.0 °C |
5000 - 6000 cP @Temperature 73.4 °F |
|
Master Bond EP30-3 High Temperature Resistant Two Component Epoxy Master Bond Polymer System EP30-3 is a two component, low viscosity epoxy featuring optical clarity and high temperature serviceability up to 450°F along with superior chemical resistance. EP30-3 h.. |
|||
Viscosity | 2400 - 6000 cP @Temperature 150 °C |
2400 - 6000 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified Product Description: Epolene C-18 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and .. |
|||
Viscosity | 2400 - 6000 cP @Temperature 150 °C |
2400 - 6000 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-18P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-18P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and .. |
|||
Viscosity | 2400 - 6000 cP @Temperature 150 °C |
2400 - 6000 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed Product Description: Epolene C-19 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and .. |
|||
Viscosity | 5000 - 6000 cP @Temperature 23.0 °C |
5000 - 6000 cP @Temperature 73.4 °F |
|
Master Bond EP34CA Low Viscosity Heat Resistant Epoxy System Master Bond EP34CA is a low viscosity, polyfunctional, heat resistant epoxy resin designed for use in high performance composite structures, potting and casting applications. EP34CA can be used up t.. |
|||
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | Part B |
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
Loctite® 222MS Low Strength/Small Screw Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
Loctite® 242 Medium Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 4000 - 6000 cP @Temperature 23.0 °C |
4000 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i.. |
|||
Viscosity | 4000 - 6000 cP @Temperature 23.0 °C |
4000 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |
|||
Viscosity | 3500 - 6000 cP @Temperature 23.0 °C |
3500 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti.. |
|||
Viscosity | 3500 - 6000 cP @Temperature 23.0 °C |
3500 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al.. |
|||
Viscosity | 3000 - 6000 cP @Temperature 23.0 °C |
3000 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® M10-D Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Viscosity | 4500 - 6000 cP | 4500 - 6000 cP | |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |
|||
Viscosity | 2000 - 6000 cP | 2000 - 6000 cP | |
3M Novec™ FC-4430 Fluorosurfactant 3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served b.. |
|||
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 50-6 |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |
|||
Viscosity | 4000 - 6000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
4000 - 6000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2060602D1 Membrane Touch Switch Paste The ink should be gently stirred before use avoiding introduction of air bubbles. It is a polymer based system for printing on polyester, PVC, etc.Can be used in membrane touch switch applicationsSc.. |
|||
Viscosity | 2000 - 6000 cP | 2000 - 6000 cP | RP-0596 |
Solvay RHODAPEX® ES-2 Surfactant Description: Primary surfactant used in shampoos, bubble baths, shin cleansers and related cosmetic products.Chemical Name: Sodium Laureth(2) SulfateCAS: 68585-34-2Available in: Asia Pacific, Europe.. |
|||
Viscosity | 3000 - 6000 cP | 3000 - 6000 cP | |
3M Novec™ FC-4432 Fluorosurfactant 3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga.. |
|||
Viscosity | 3500 - 6000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500 - 6000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2010309P3 Platinum Paste This product has been designed as a platinum paste suitable for high temperature firing applications on to electro-ceramic substrates such as NTC. It is capable of withstanding repeated firing at h.. |