Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3000 - 3500 cP | 3000 - 3500 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 46-73/32 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa |
|||
Viscosity | 1500 - 3500 cP @Temperature 25.0 °C |
1500 - 3500 cP @Temperature 77.0 °F |
Kinematic of 5.25% solution in Toluene |
Sibur DST-30R-01 3rd Group Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE) Kraton D 1184, 1186. As modifiers for bitumen for production of roofing materials, footwear compositions, adhesives, and coverings, as well as for modification of plastics. Addition of thermal ela.. |
|||
Viscosity | 1100 - 3500 cP | 1100 - 3500 cP | Dynamic |
Dow Corning Emulsifier 10 Emulsifier Emulsifier designed to prepare water-in-oil and water-in-silicone emulsions for use in skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning |
|||
Viscosity | 2000 - 3500 cP @Temperature 23.0 °C |
2000 - 3500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H31LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31LV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electron.. |
|||
Viscosity | 2900 - 3500 cP @Temperature 60.0 °C |
2900 - 3500 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G216 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 200 - 3500 cP | 200 - 3500 cP | Average value: 1830 cP Grade Count:12 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Viscosity | 1300 - 3500 cP | 1300 - 3500 cP | |
Huntsman Araldite GZ 488 V-32 US Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 3570 to 5500. Max color is 3.Comments/Applications: Very high molecular weight solid epoxy (8,000 - 10,000), 35% solids in PM acetate. Outstanding adhesion, excellen.. |
|||
Viscosity | 2000 - 3500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
2000 - 3500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2000802P2 Carbon Graphite Ink This product is designed to be used for screen-printing working electrodes. This ink has been optimized to give superior electrochemical performance. It combines good line definition and good electr.. |