Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1600 - 3000 cP | 1600 - 3000 cP | Thixotropic |
ND Industries StudGrade® 131 Permanent CT Threadlocker General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 25.0 °C |
2000 - 3000 cP @Temperature 77.0 °F |
|
Northstar Polymers MPC-026 Isocyanate prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 2000 - 3000 cP @Temperature 25.0 °C |
2000 - 3000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV620 UV-curable Adhesive PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 25.0 °C |
2000 - 3000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV670 UV-curable Adhesive PERMABOND UV670 is a single part, fast curing, UV curable adhesive. The cured adhesive is tough, flexible and has excellent impact resistance. Permabond UV670 is well suited for bonding glass to met.. |
|||
Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1116 A (SBS) Radial Triblock Copolymer Description: Kraton D1116 A is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified: Kraton.. |
|||
Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1116 E (SBS) Radial Triblock Copolymer Description: Kraton D1116 E is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified: Kraton.. |
|||
Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | |
Lucite International Colacryl ® 1205 Acrylic Solution Resin Butyl Methacrylate polymers are more flexible and softer than Methyl Methacrylate types. The polymers are compatible with nitrocellulose, chlorinated rubber, some phenolics and maleics. Butyl methac.. |
|||
Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | 20% Toluene Solution at 25°C; BAM 922 |
Kraton® D1116 K (SBS) Radial Triblock Copolymer Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified.. |
|||
Viscosity | 2500 - 3000 cP | 2500 - 3000 cP | As Supplied |
Heraeus Cleviosâ„¢ S V3 Antistatic/Conductive Polymer Coating for Screen Printing Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Cleviosâ„¢ S V3 grade .. |
|||
Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | Part A |
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 23.0 °C |
2000 - 3000 cP @Temperature 73.4 °F |
|
Master Bond EP30FL Low Viscosity, Flexibilized Two Component Epoxy Master Bond Polymer System EP30FL is a low viscosity, flexibilized, two component epoxy resin system for high performance potting, casting, encapsulation as well as bonding and sealing. Master Bond .. |
|||
Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | Part B |
Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excel.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 23.0 °C |
2000 - 3000 cP @Temperature 73.4 °F |
|
Master Bond EP39-2 Fast Curing Optically Clear Two Component Epoxy System Master Bond Polymer System EP39-2 is a fast curing, low viscosity, optically clear two component epoxy system for high performance bonding, sealing, coating and casting. It is 100% reactive and does.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 23.0 °C |
2000 - 3000 cP @Temperature 73.4 °F |
|
Master Bond EP30M3LV Electrically Insulative, Low Viscosity Two Component Epoxy Master Bond Polymer System EP30M3LV is a lower viscosity, two component epoxy system for high performance bonding, sealing and encapsulation. It is formulated to cure at ambient temperatures or mor.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 23.0 °C |
2000 - 3000 cP @Temperature 73.4 °F |
|
Master Bond EP31 High Shear and Peel Strength Room Temperature Curing Epoxy Master Bond Polymer System EP31 is a two component room temperature curing epoxy for high performance structural bonding applications featuring lap shear strengths exceeding 4600 psi. In addition, u.. |
|||
Viscosity | 1000 - 3000 cP @Temperature 23.0 °C |
1000 - 3000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Viscosity | 1500 - 3000 cP @Temperature 23.0 °C |
1500 - 3000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Viscosity | 1500 - 3000 cP @Temperature 23.0 °C |
1500 - 3000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di.. |
|||
Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | dynamic |
Dow Corning 2-2078 FLUID A liquid amino phenyl silicone resin primarily for use in hair care products, but has utility in color cosmetics as well.Information provided by Dow Corning |
|||
Viscosity | 500 - 3000 cP @Temperature 25.0 °C |
500 - 3000 cP @Temperature 77.0 °F |
spindle n 3-10 RPM; MA143LFE |
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 35.0 °C |
2000 - 3000 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® F 3 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 2000 - 3000 cP @Temperature 35.0 °C |
2000 - 3000 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® Lp 2500_30 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 2000 - 3000 cP @Temperature 35.0 °C |
2000 - 3000 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | mixed |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |
|||
Viscosity | 500 - 3000 cP @Shear Rate 1.00e+10 1/s, Temperature 20.0 °C |
500 - 3000 cP @Shear Rate 1.00e+10 1/s, Temperature 68.0 °F |
|
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane Solution NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and d.. |
|||
Viscosity | 1500 - 3000 cP @Temperature 35.0 - 35.0 °C |
1500 - 3000 cP @Temperature 95.0 - 95.0 °F |
Average value: 2380 cP Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |