Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 100 - 15000 cP @Temperature 45.0 - 82.2 °C |
100 - 15000 cP @Temperature 113 - 180 °F |
Average value: 2520 cP Grade Count:8 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Viscosity | 6000 - 15000 cP | 6000 - 15000 cP | |
Huntsman Araldite GZ 7071 PM-75 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 450 to 575. Max color is 3.Comments/Applications: GT 7071 - 75% solids in PM (propylene glycol monomethyl ether.) High performance 2-package systems for coatings, fl.. |
|||
Viscosity | 13000 - 15000 cP | 13000 - 15000 cP | |
Huntsman MY 9634 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: Narrow viscosity MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistan.. |
|||
Viscosity | 10000 - 15000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
10000 - 15000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2020322D6 Platinum Polymeric Ink C2020322D6 is a screen printable Platinum ink designed for printing working electrodes in electrochemical sensor applications. The paste can be used to detect H2O2, is suitable for developing biose.. |
|||
Viscosity | 12000 - 15000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
12000 - 15000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2050106D7 Carbon Graphite Ink This Carbon Graphite Ink is designed to be used for screen printing working electrodes. This is an ink which has been optimized to give superior electrochemical performance. It gives excellent elec.. |
|||
Viscosity | 8000 - 15000 cP @Temperature 40.0 °C |
8000 - 15000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PPG CPU-2095 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 10000 - 15000 cP | 10000 - 15000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A8510 TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Viscosity | 10000 - 15000 cP | 10000 - 15000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A8521 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Viscosity | 7500 - 15000 cP | 7500 - 15000 cP | 540MA3C52 |
Solvay MIRAPOL® 550 P Surfactant Description: Mirapol 550 P can be used effectively in shampoos and conditioners at typical use levels of 0.5% (copolymer solids) to provide excellent lubricity, softeness light hair conditioning and.. |
|||
Viscosity | 7500 - 15000 cP | 7500 - 15000 cP | #4 SP @ 10 rpm; RP-0596 |
Solvay MIRAPOL® 550 Surfactant Description: Cationic polymer providing good wet/dry combability properties. Imparts smooth feel, anti-static, luster and detangling properties to the hair and silky feel to the skin. Stabilizes foa.. |
|||
Viscosity | 10000 - 15000 cP @Temperature 23.0 °C |
10000 - 15000 cP @Temperature 73.4 °F |
|
Master Bond EP21AR Acid Resistant Two Component Epoxy Master Bond EP21AR is a two component epoxy resin compound for durable, high performance, coating liner and adhesive/sealant with outstanding acid as well as excellent overall chemical resistance. E.. |
|||
Viscosity | 11000 - 15000 cP | 11000 - 15000 cP | Part B |
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien.. |
|||
Viscosity | 9000 - 15000 cP | 9000 - 15000 cP | Part A |
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 12000 - 15000 cP | 12000 - 15000 cP | |
Master Bond Mastersil 150 Two Part, Condensation Cured, Flexible Silicone Master Sil 150 is a 2 part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation.. |
|||
Viscosity | 12000 - 15000 cP | 12000 - 15000 cP | Dynamic |
Dow Corning XIAMETER® PMCPOHX-4040 Polymer 14000CS Is chemically equivalent to DOW CORNING® 3-0084 POLYMER. Polydimethylsiloxane polymer with terminated, curable silanol functionality.Information provided by Dow Corning |
|||
Viscosity | 9000 - 15000 cP @Temperature 23.0 °C |
9000 - 15000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Viscosity | 9000 - 15000 cP @Temperature 23.0 °C |
9000 - 15000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Viscosity | 10000 - 15000 cP @Temperature 23.0 °C |
10000 - 15000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® H31D-LV Epoxy Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i.. |
|||
Viscosity | 9000 - 15000 cP @Temperature 23.0 °C |
9000 - 15000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica.. |
|||
Viscosity | 9000 - 15000 cP @Temperature 23.0 °C |
9000 - 15000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientif.. |
|||
Viscosity | 10000 - 15000 cP | 10000 - 15000 cP | |
Beijing Ranger Chem 0164E Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 5000 - 15000 cP | 5000 - 15000 cP | |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Viscosity | 11500 - 15000 cP | 11500 - 15000 cP | |
Beijing Ranger Chem SM-828 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 12000 - 15000 cP | 12000 - 15000 cP | |
Beijing Ranger Chem SM-828CA Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 11500 - 15000 cP | 11500 - 15000 cP | |
Beijing Ranger Chem SM-828H Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 13000 - 15000 cP | 13000 - 15000 cP | |
Beijing Ranger Chem SM828R Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 8000 - 15000 cP | 8000 - 15000 cP | |
Beijing Ranger Chem SM-601RX75 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 10000 - 15000 cP | 10000 - 15000 cP | |
Lucite International Colacryl ® TS1171 Acrylic Solution Resin Butyl methacrylate-Methyl methacrylate copolymerThis product is a fairly soft and flexible copolymer with reasonable abrasion resistance. It has good UV resistance and is therefore suitable for outd.. |