Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 70 - 90 cP @Temperature 25.0 °C |
70 - 90 cP @Temperature 77.0 °F |
Uncured |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Viscosity | 70 - 90 cP @Temperature 25.0 °C |
70 - 90 cP @Temperature 77.0 °F |
Uncured |
Permabond 102 Cyanoacrylate, General purpose PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano.. |
|||
Viscosity | 70 - 90 cP @Temperature 25.0 °C |
70 - 90 cP @Temperature 77.0 °F |
Uncured |
Permabond 920 Cyanoacrylate, High temperature PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB.. |
|||
Viscosity | 70 - 100 cP | 70 - 100 cP | |
Huntsman AroCy L-10 Cyanate Ester Comments/Applications: Max color is 8. Lowest viscosity liquid cyanate ester. Used in filament winding, RTM, pultrusion. Can also be used as a viscosity modifier in other cyanate ester systems.Da.. |
|||
Viscosity | 70 cP | 70 cP | |
KKPC KOSYN KSL 203 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro.. |
|||
Viscosity | 70 cP | 70 cP | |
KKPC KOSYN KSL 201 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro.. |
|||
Viscosity | 70 cP | 70 cP | B-type viscometer (60rpm) |
Mitsui UNISTOLEâ„¢ R-120K Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Viscosity | 70 - 130 cP | 70 - 130 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-120 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Viscosity | 70 - 130 cP | 70 - 130 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-120L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Viscosity | 70 cP @Temperature 25.0 °C |
70 cP @Temperature 77.0 °F |
|
Shin-Etsu Silicones Primer 33 Primer No. 33 is a reddish brown colored primer designed for bonding HCR/silicone rubber to plastics and metals such as aluminum, stainless steel, and iron. Use: Metal substratum surface must be cl.. |
|||
Viscosity | 70 - 120 cP | 70 - 120 cP | |
Master Bond UV15LV One Component, UV Curable Epoxy Based System Product Description: Master Bond UV15LV is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It has low viscosity and it is widely used in a variety of .. |
|||
Viscosity | 70 - 80 cP @Temperature 20.0 °C |
70 - 80 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-75 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 70 - 120 cP | 70 - 120 cP | HY2954 cycloaliphatic amine hardener; DIN 53015 |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Viscosity | 70 cP | 70 cP | dynamic |
Dow Corning TM-1950 EMULSION Dow Corning® TM-1950 Emulsion and Dow Corning® TM-1951 Emulsion are water-based silicone products with excellent dilution stability, which provide release of tissue paper from felt, fabric and wir.. |
|||
Viscosity | 70 cP | 70 cP | |
Dow PAPI™ 95 Polymeric MDI PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan.. |
|||
Viscosity | 70 - 130 cP | 70 - 130 cP | |
3M Scotch-Weld™ CA8 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3.. |
|||
Viscosity | 70 cP @Temperature 70.0 °C |
70 cP @Temperature 158 °F |
at 100/28 (50-6/50-17) pbw |
Abatron AboCast 50-6/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months. |
|||
Viscosity | 70 - 120 cP | 70 - 120 cP | |
3M Pronto™ CA-8 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Fast setting adhesive with exce.. |
|||
Viscosity | 70 cP | 70 cP | |
BASF Lupranate® M10 Isocyanate Description: Lupranate® M10 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate M10 Isocyanate is a polymeric MDI which contains a relatively high level .. |