Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3600 - 4400 cP | 3600 - 4400 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 190 (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 3600 - 5000 cP | 3600 - 5000 cP | |
Huntsman MY 721 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 109 to 117. Color: BrownComments/Applications: Lowest viscosity, tetra-functional epoxy with the same chemistry as MY 720. Used for high performance composites, adhe.. |
|||
Viscosity | 3600 - 4200 cP | 3600 - 4200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-626SH TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 3600 - 4600 cP @Time 7200 sec |
3600 - 4600 cP @Time 2.00 hour |
RP-0891 |
Solvay JAGUAR® HP 8 COS Surfactant Description: Hydroxypropyl Guar for thickening, which provides a fluid and smooth wet feel to formulationsChemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: Hydroxypropyl GuarCAS: 39421-75-5S.. |
|||
Viscosity | 3600 cP | 3600 cP | Mixed |
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai.. |
|||
Viscosity | 3600 cP | 3600 cP | dynamic |
Dow Corning SE 4440 LP KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, low viscosity.Information provided by Dow Corning |
|||
Viscosity | 3600 cP @Temperature 180 °C |
3600 cP @Temperature 356 °F |
ETM 22-31 |
ExxonMobil ESCOREZ™ 5340 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Viscosity | 3600 cP @Temperature 25.0 °C |
3600 cP @Temperature 77.0 °F |
|
Cytec (Conap) FR-1046 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 3600 cP @Temperature 25.0 °C |
3600 cP @Temperature 77.0 °F |
|
Cytec (Conap) FR-1047 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 3600 - 4400 cP @Temperature 35.0 °C |
3600 - 4400 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G217 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 3600 cP | 3600 cP | Uncured |
Atom Adhesives AA-BOND 201 Epoxy Adhesive AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system.. |
|||
Viscosity | 3600 - 4400 cP @Temperature 35.0 °C |
3600 - 4400 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G205 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |