Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2000 cP | 2000 cP | |
Resin Technology Group 15 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 15 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 2000 - 3000 cP @Temperature 25.0 °C |
2000 - 3000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV620 UV-curable Adhesive PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I.. |
|||
Viscosity | 2000 cP | 2000 cP | Mixed |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
Viscosity | 2000 cP | 2000 cP | |
NextGen Adhesives G907-08 Epoxy Adhesive Description: NGAC G907-08 is a low viscosity, electrically insulating, heat cured and 2-part adhesive systems designed for applications where temperature and chemical resistance is critical. The NGA.. |
|||
Viscosity | 2000 cP | 2000 cP | |
Resinlab® CYNERGY CA6207 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | |
Huntsman MY 0500 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 105 to 115. Max color is 11.Comments/Applications: Trifunctional low viscosity epoxy resin based on para amino phenol. Performance upgrader for bisphenol A resins. .. |
|||
Viscosity | 2000 cP | 2000 cP | |
Lord Adhesives 9900 Normal Setting, High Viscosity, Odorless, Non-Frosting Methyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1116 E (SBS) Radial Triblock Copolymer Description: Kraton D1116 E is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified: Kraton.. |
|||
Viscosity | 2000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
2000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2050905D3 80:20 Silver Palladium Ink C2050905D3 is an ink based on a 80:20 ratio of Silver:Palladium; a screen printing internal electrode ink for flexible PZT components. This Material is compatible with PVB tape. The ink is designed .. |
|||
Viscosity | 2000 cP | 2000 cP | |
Shin-Etsu Silicones KE-1204 BL Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | <= 2000 cP | <= 2000 cP | #3 SP @ 12 rpm |
Solvay MACKANATE® OPV-N Surfactant Product Description: Mackanate OPV-N is a vegetable derived, amido type monoester sulfosuccinate. It is a high foaming surfactant, mild to both eyes and skin with thickening properties. Mackanate OP.. |
|||
Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | Part A |
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no.. |
|||
Viscosity | <= 2000 cP | <= 2000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1052-30 Nitrile Elastomer Nipol 1052-30 is a copolymer of butadiene and acrylonitrile with medium oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Low Mooney versi.. |
|||
Viscosity | 2000 - 5000 cP | 2000 - 5000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1051 Nitrile Elastomer Nipol 1051 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Easy processing version of Ni.. |
|||
Viscosity | 2000 - 10000 cP | 2000 - 10000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1432T Nitrile Powder and Crumb Elastomer Nipol 1432T is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile content. Sufficient antioxidant is added during manufacture for normal storage conditions.Used in adhesives and.. |
|||
Viscosity | 2000 - 10000 cP | 2000 - 10000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1442 Nitrile Powder and Crumb Elastomer Nipol 1442 is a copolymer of butadiene and acrylonitrile with medium-high acrylonitrile content. Nipol 1442 shall be in the form of nominal 1/4" three-dimensional chips containing approximately 5%mi.. |
|||
Viscosity | 2000 - 4100 cP @Temperature 23.0 °C |
2000 - 4100 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® E3001 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
Viscosity | 2000 - 3500 cP @Temperature 23.0 °C |
2000 - 3500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H31LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H31LV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electron.. |
|||
Viscosity | 2000 - 3000 cP @Temperature 35.0 °C |
2000 - 3000 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 2000 cP | 2000 cP | "A" component |
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par.. |
|||
Viscosity | 2000 cP | 2000 cP | Uncatalyzed, QM 245B |
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Viscosity | 2000 cP | 2000 cP | |
Abatron AboCast 8110-6/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Viscosity | 2000 cP | 2000 cP | A Component; Spindle #3; speed 10 rpm; ASTM D1824 |
Aptek 6106-A/B Epoxy Encapsulant and/or Potting Compound Optoelectronic grade encapsulant/potting compound – will not attack/cloud polysulphone casings. Lower Tg version, APTEK 6110-A/B, available for ceramic blob-top applications.Part A is hazy blue. Pa.. |
|||
Viscosity | 2000 - 2500 cP | 2000 - 2500 cP | Brooksfield LV Viscometer |
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | mixed |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |