Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Viscosity | 2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin
(discontinued **) Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Viscosity | 2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Viscosity | 2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Viscosity | 2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Elvax® 3165 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3165 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Viscosity | 2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 240 °C |
2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 464 °F |
|
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® XP32-E1 PA6 Film Extrusion, Medium Viscosity, Lubricated, Nucleated |
|||
Viscosity | 2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
2.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® XP36-E1 PA6 Film Extrusion, Medium Viscosity, Nucleated, Lubricated |
|||
Viscosity | 2.00e+6 - 2.60e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
2.00e+6 - 2.60e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Viscosity | 2.00e+6 - 2.50e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
2.00e+6 - 2.50e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR® 2751-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |
|||
Viscosity | 2.00e+6 - 2.50e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
2.00e+6 - 2.50e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |