Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 170 cP @Temperature 25.0 °C |
170 cP @Temperature 77.0 °F |
of Solution, 5% wt/wt in Styrene |
Polimeri Europa Intene® 50 (A-AM-AF) Butadiene Rubber Intene® 50 A-AF-AM are solution polymerized low cis polybutadiene produced using an alkyl lithium catalyst. A food contact approved, non-staining antioxidant is added during the production process.. |
|||
Viscosity | 170 cP @Shear Rate 1000 1/s, Temperature 400 °C |
170 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Viscosity | 170 - 110000 cP @Temperature 40.0 - 175 °C |
170 - 110000 cP @Temperature 104 - 347 °F |
Average value: 13800 cP Grade Count:12 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 170 cP | 170 cP | |
KKPC KOSYN KSL 102 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force.Applications: Carpet Backing, Adhesive .. |
|||
Viscosity | 170 cP | 170 cP | |
Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 19°C. Average solids: 60%. Usage Notes: Use with IMI 74010 hardener for final coat over field coils, windings, and heavy duty motors. |
|||
Viscosity | 170 cP | 170 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 160 Coating Example of a typical SL 100/SL 200 blend; low release at high speeds; medium-low viscosityInformation provided by Dow Corning |
|||
Viscosity | 170 cP | 170 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 560 Coating Information provided by Dow Corning |
|||
Viscosity | 170 cP | 170 cP | dynamic |
Dow Corning SYL-OFF® SL 160 COATING Example of a typical SL 100/SL 200 blend; low release at high speeds; medium-low viscosityInformation provided by Dow Corning |
|||
Viscosity | 170 cP | 170 cP | dynamic |
Dow Corning SYL-OFF® SL 560 COATING Information provided by Dow Corning |
|||
Viscosity | 170 cP | 170 cP | 5% Styrene Solution; ASTM D445 |
Chi Mei Kibipol® PR-225 Butadiene Rubber (LBR) Plastic modifier |
|||
Viscosity | 170 - 210 cP @Temperature 60.0 °C |
170 - 210 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G680 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 170 - 230 cP @Temperature 25.0 °C |
170 - 230 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT CR-30-20 MDI Isocyanate Description of product: Polymethylene-polyphenyl-isocyanate, 4,4-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers.Field of application: With suitable.. |
|||
Viscosity | 170 - 230 cP @Temperature 25.0 °C |
170 - 230 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT CR30-20/LA MDI Isocyanate Description of product: Polymethylene-polyphenyl-isocyanate, 4,4`-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers. Field of application: With suitab.. |