Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 100 - 200 cP | 100 - 200 cP | |
ND Industries 600 Methacrylate Resin Activator Activator for structural Adhesives and anaerobics. Solvent free. |
|||
Viscosity | 100 cP | 100 cP | |
Resinlab® CYNERGY CA6103 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 100 cP | 100 cP | |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Viscosity | 100 cP | 100 cP | Part A (Isocyanate), RVT, #2, 20 rpm; TM R050-12 |
Resinlab® UR3001HP Black Urethane Encapsulant Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e.. |
|||
Viscosity | 100 cP | 100 cP | |
Resinlab® CYNERGY CA6805 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 100 cP | 100 cP | Fed Std Method 4287 |
Humiseal 1A20LSE Urethane Conformal Coating Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses ther.. |
|||
Viscosity | 100 - 110 cP | 100 - 110 cP | |
Huntsman DT 3126-2 Epoxy Accelerator Comments/Applications: Granular solid. Powder coating accelerator for epoxy/COOH functional polyesters, used at 2-3% levels.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has be.. |
|||
Viscosity | 100 - 180 cP | 100 - 180 cP | |
LG Chemical CP-HR Polycarboxylic Copolymer Description: Advantages: CP-HR is the main raw material for concrete admixture, which improves water reducing ability of Ultra high strength concrete. CP-HR exhibits superior properties of High stor.. |
|||
Viscosity | 100 - 250 cP | 100 - 250 cP | As Supplied |
Heraeus Cleviosâ„¢ P HC V4 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P HC V4 is an antistatic material based on PED.. |
|||
Viscosity | 100 - 200 cP | 100 - 200 cP | As Supplied |
Heraeus Cleviosâ„¢ P T2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P T2 is an antistatic material based on PEDOT:.. |
|||
Viscosity | <= 100 cP | <= 100 cP | |
Solvay Specialty Polymers Solvera® PT 5045 PFPE Surface Treatment Solvera® PFPE is a sustainable surface treatment developed to increase the grease resistance of paper packaging, pizza boxes, popcorn bags, pet food bags and food wraps. Both solvent and aqueous.. |
|||
Viscosity | 100 cP @Temperature 25.0 °C |
100 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 100 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | 100 - 150 cP | 100 - 150 cP | Part B |
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p.. |
|||
Viscosity | 100 - 110 cP | 100 - 110 cP | mixed compound; thixotropic |
Master Bond MB250NT Low viscosity ethyl cyanoacrylate Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi.. |
|||
Viscosity | 100 - 140 cP | 100 - 140 cP | RTM 120 bisphenol epoxy resin containing reactive diluent; DIN 53015 |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Viscosity | 100 - 200 cP | 100 - 200 cP | NOV QC 020 |
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 100 - 200 cP @Temperature 23.0 °C |
100 - 200 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
Viscosity | 100 cP | 100 cP | |
ACC EP MAP-18 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-18 contains 18% NCO. Pa.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT BLUE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT RED 3 |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT BLUE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT RED 3 |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 100 - 250 cP | 100 - 250 cP | |
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95% This carbon and graphite based coating is formulated for parting of aluminum permanent molds, non-sticking in glass forming applications, and lubrication and stop-off in metalworking and wire drawin.. |
|||
Viscosity | <= 100 cP | <= 100 cP | |
3M Dynamar™ RC 5115 Rubber Curative 3M™ Dynamar™ Rubber Curatives RC 5105, RC 5110, RC 5115, RC 5120 and RC 5125 are liquid curatives that offer fast and easy incorporation into solvent based FKM solution coatings. RC 5115 is 50% bi.. |
|||
Viscosity | 100 cP | 100 cP | Part A (Isocyanate), RVT, #2, 20 rpm; TM R050-12 |
Resinlab® UR3001HP Clear Urethane Encapsulant Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e.. |