Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |
|||
Melt Index of Compound | 2.5 - 4.0 g/10 min | 2.5 - 4.0 g/10 min | |
Sibur 21030 Polypropylene Compounding for stabilization 16K, 16V, 16N, 16M, 16H superior quality. For production of technical and domestic products of complicated profile, of non-woven materials. |
|||
Melt Index of Compound | 2.5 - 4.0 g/10 min | 2.5 - 4.0 g/10 min | |
Sibur 21030-PM1 Polypropylene with Low Haze For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products. |
|||
Melt Index of Compound | 3.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |