Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 19 g/10 min @Load 5.00 kg, Temperature 260 °C |
19 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY8540 PC+ABS (Europe-Africa-Middle East) CYCOLOY CY8540 is a PC+ABS blend, especially designed for textile backmolding in automotive interior applications. High flow grade, which allows low temperature processing to maintain fabric integri.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 300 °C |
19 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Asia Pacific) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Melt Index of Compound | 19 g/10 min @Load 3.80 kg, Temperature 300 °C |
19 g/10 min @Load 8.38 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DEL32P PC (Asia Pacific) LNP* Stat-kon* DEL32P is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |
|||
Melt Index of Compound | 19 g/10 min @Load 2.16 kg, Temperature 300 °C |
19 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific) LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A .. |
|||
Melt Index of Compound | 19 g/10 min @Load 2.16 kg, Temperature 250 °C |
19 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Melt Index of Compound | 19 g/10 min @Load 5.00 kg, Temperature 280 °C |
19 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Melt Index of Compound | 19 g/10 min @Load 5.00 kg, Temperature 280 °C |
19 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Melt Index of Compound | 19 g/10 min @Load 5.00 kg, Temperature 280 °C |
19 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Melt Index of Compound | 19 g/10 min @Load 10.0 kg, Temperature 280 °C |
19 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East) NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306. |
|||
Melt Index of Compound | 19 g/10 min @Load 2.16 kg, Temperature 260 °C |
19 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 19 g/10 min @Load 1.20 kg, Temperature 224 °C |
19 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |