Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.7 - 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 - 2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Melt Index of Compound | 1.7 - 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 - 2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Melt Index of Compound | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
Melt Index of Compound | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc.. |
|||
Melt Index of Compound | 1.7 g/10 min @Temperature 230 °C |
1.7 g/10 min @Temperature 446 °F |
ASTM D1238 |
Mitsui ADMER® QB520A PP Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t.. |