Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm @Thickness 3.17 mm |
0.0020 - 0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-61/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm @Thickness 6.35 mm |
0.0020 - 0.0030 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |