Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0050 - 0.0060 cm/cm @Thickness 3.17 mm |
0.0050 - 0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm @Thickness 3.00 mm |
0.0050 - 0.0080 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |