Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00200 - 0.100 cm/cm
0.00200 - 0.100 in/in
Average value: 0.0150 cm/cm Grade Count:30
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage, Transverse 0.00500 - 0.100 cm/cm
0.00500 - 0.100 in/in
Average value: 0.0118 cm/cm Grade Count:62
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage, Transverse 0.00680 - 0.100 cm/cm
0.00680 - 0.100 in/in
Average value: 0.0157 cm/cm Grade Count:24
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..